Diagnose and resolve common media wear issues — including premature breakdown, glazing, and incorrect consumption rates.
Normal vs abnormal media wear
All finishing media wears down over time — this is normal and expected. As media wears, the abrasive particles within it are continuously exposed, maintaining cutting action. However, abnormal wear patterns indicate a process problem that needs addressing.
Common media wear problems
Premature breakdown
If media is breaking into small fragments or wearing down much faster than expected, the likely causes are:
- Bowl amplitude set too high — reduce amplitude
- Load ratio too low — too many components, not enough media causing impact forces
- Wrong media type for the application — media too soft for the cut required
- Compound pH incorrect — some compounds are corrosive to certain media binders
Media glazing
Glazed media feels smooth and has lost its cutting ability. The surface has become polished rather than abrasive. Causes include:
- Compound flow rate too high — excessive lubrication prevents abrasive action
- Cycle time too long without compound — media surfaces become burnished
- Wrong compound for the media type
Quick check: Rub a piece of media against a piece of mild steel. You should feel a definite cutting action. If the media slides smoothly with no abrasion, it is glazed and needs replacing.
Media loading (part material embedding into media)
This occurs when workpiece material — particularly soft metals like aluminium or copper — becomes embedded in the media surface, smearing and staining components. Solutions:
- Use a compound specifically formulated for the material being processed
- Ensure compound flow rate is adequate
- Reduce cycle time and check results at shorter intervals
When to replace media
Replace media when it has worn down to approximately 50% of its original size, or when cut rate has noticeably reduced even after compound and amplitude adjustments. Keep a log of media top-up quantities — a sudden increase in consumption indicates a process problem.
Not finding what you need?
Our technical team has over 50 years of hands-on experience. Call us or request a free sample trial.